Paint was quite dull, there was loads of contaminants stuck to it so claying took quite a while. p.s. can the clay bar be reused? Paint is now quite shiny and smooth now though.
Anyway all the panels have got swirl marks on, i dont think its been polished properly much if ever
Yes you can reuse the clay a number of times providing that you can find clean surfaces by folding it a few times. You just knead the clay and fold the dirty surfaces into itself to reveal a clean area.
If the panels have swirls and and scratches then I would definitely use a polish first as a glaze will have little effect. You can use a glaze afterwards for a deeper depth of shine although it isn't really necessary. Then apply a wax or sealant to protect your efforts.
Cheers. To add further confusion a lot of the sellers on ebay in their descriptions state that the sealant glaze polish will get rid of fine swirls and scratches
I used the megs polish but as Steve said, it wasnt harsh enough to cut through the paint.
Would the menzerna intensive polish be the correct one to use? Also is scratch-x any good?
Menzerna Intensive will be fine although you will need to follow this up with Menzerna Final Finish to get the results you want. Will you be using a machine polisher as you'll really need one. I've never used scratch-X myself I'm afraid.
Scratch-X is damn good - I've used on places like under door handles where finger nails cause isolated surface scratches... Don't think it would be good for a big swirly surface like a panel or door. Thats for a decent cutting compound and the other PC. Ask for advice on which compounds to try. Can be done by hand but its boring as fook.
Sal check out megs pro range ,the bottle shows you how much cut it has ,1\10 ,
I use megs 83 alot this has medium cut 5\10 but also contains polishing agents which give a great shine and is easy to work with ,use on a megs cutting or polishing pad
depending on the correction needed ,use the softest first ,then wax to seal the paint.
We process personal data about users of our site, through the use of cookies and other technologies, to deliver our services, personalize advertising, and to analyze site activity. We may share certain information about our users with our advertising and analytics partners. For additional details, refer to our Privacy Policy.
By clicking "I AGREE" below, you agree to our Privacy Policy and our personal data processing and cookie practices as described therein. You also acknowledge that this forum may be hosted outside your country and you consent to the collection, storage, and processing of your data in the country where this forum is hosted.